Surface analysis

Mercury porosimetry

Analyte:

  • Solid samples with or without pores/cavaties
  • Samples must be dry
  • 0.5 – 1 g sample material (dependent of porosity)

 

Equipment:

Mercury porosimeter composed of :

  • Pascal 140 with pressure range between 0.013 bis 0.4 MPa of determination of macro pores and
  • Pascal 440 with pressure range between 0.1 bis 400 MPa of determination of meso pores
    (Fa. Thermo Electron Corporation, Milano, Italy)

 

Evaluation methods and targets:

  • Determination of cumulative pore volume of measurement range
  • Determination of pore diameters und –distribution (registration of pores between 4 nm and 116,000 nm diameter)
  • Calculation of porosity und density
  • Calculation of specific surface taking as a basis different models of pores
  • Determination of particle size and -distribution between 0.01 and 330 µm

 

Application examples:

  • Determination of cumulative pore volume, pore diameter anddistribution of porous bead cellulose
  • Determination of cumulative pore volume, pore diameter and
  • Distribution of foamed chitosan
  • Determination of cumulative pore volume, pore diameter and
  • Distribution of concrete